Sciencemadness Discussion Board
more gold refining questions a quick introduction to my question; I soaked scrap cpus and a few gold plated pins in 36% HCl and got Solution A, After rinsing I added 69% HNO3 to the scrap and got Solution B After rinsing I added Aqua Regia (freshly mixed, 26 ml 69% HNO3 added to 100 ml 36 % HCl). This is a photo of the Aqua Regia 'refluxing'